| Color: |
Aluminum or Off-White |
Tensile:
ASTM D-412
Strength:
Elongation: |
1600 psi 100 psi (11 ± .69 MPa)
180% 10% |
| Tear Resistance: |
ASTM D-624 Die C 210 ± 5 pli (37.5 ± 0.9 kg/cm) Lb. / in |
| Hardness |
ASTM D-2240 80 - 3 Shore A |
| Water Absorption: |
ASTM D-471 2.5% Maximum 7 days, R.T. |
| Water Vapor Permeability: |
ASTM E-96 Procedure BW 0.02 Perm Inches (.51 mm)
100% R.H. Difference @ 23°C |
| Toxicity |
Part B contains polymeric diisocyanate, which is toxic if heated in a confined area or inhaled as particulate matter. An air supply respirator is required for spray applications and containers of Part B should not be heated above 120°F (49°C). However, heating of either component to 140°F (60°C) is acceptable when using plural component spray equipment. |
| Adhesion: |
Adheres well to polyurethane foam, modified bitumen, and other roof substrates. It is recommended that FAST SET URETHANE 530 be applied in a single pass. |
| Coverage: |
Sq. Ft./Gal./Mil: 1528 (37.4 m2 / L / .025 mm) |
| Solids: |
| Part A (Poly) |
Part B (Iso) |
| Weight: 100% |
94.1 % |
| Volume: 100% |
90.6 % |
|
| Flash Point: |
Part A (poly): NONE
Part B (iso): 73.8 g/L
> 100°F (>38°C) |
| Storage Stability: |
Part A: One year at 75°F to 95°F (24°C to 35°C)
Part B: Six months at 75°F to 95°F (24°C to 35°C) |
| Thinner: |
Do not thin. |
| Cure: |
Applied coating will cure in 24 hours with 70ºF (21ºC) and 40% relative humidity. Lower temperatures and humidity will require longer times to cure. |
| Clean Up: |
Spray equipment may be cleaned with T-5112 thinner. |